杭州九朋新材料有限责任公司
咨询热线 13235718865
 
纳米氟化镁
  • 品牌:九朋
  • 产地:浙江
  • 型号:1kg
  • 货号:12121
  • 纯度:99.9
  • cas:7783-40-6
  • 价格: ¥350/千克
  • 发布日期: 2026-04-08
  • 更新日期: 2026-09-21
产品详请
产地 浙江
品牌 九朋
货号 12121
用途 固态电池
包装规格 1kg
CAS编号 7783-40-6
纯度 99.9%
是否进口

纳米氟化镁

产品名称:氟化镁(别名:二氟化镁)
CAS 号:7783-40-6

技术指标

型号 CY-FHM30
外观 浅灰色粉末
粒径(nm) 30–50
比表面积(m²/g) 100–150

应用领域

  • 用作冶炼金属镁的助溶剂、电解铝的添加剂、光学透镜镀膜材料、钛颜料的涂着剂、阴极射线屏的荧光材料等

  • 用于光学玻璃、陶瓷工业及电子工业

  • 用于制造陶器、玻璃,作为冶炼镁的助溶剂,以及光学仪器镜头和滤光器的涂层、光学透镜的反折射剂和焊接剂

  • 固态电池:氟化镁可作为固态电解质的功能添加剂或界面修饰层材料,有助于降低界面阻抗、控制锂枝晶生长、提高固态电池的循环稳定性和安全性。其在宽电化学窗口下表现稳定,适用于高电压固态电池体系。

包装方式

样品包装:100 g/袋、500 g/袋 或 1 kg/袋

储存条件

保持密封,存放于阴凉、干燥处,避免受潮。


Nano Magnesium Fluoride

Product Name: Magnesium Fluoride (also known as Magnesium Difluoride)
CAS No.: 7783-40-6

Technical Specifications

Model CY-FHM30
Appearance Light gray powder
Particle Size (nm) 30–50
Specific Surface Area (m²/g) 100–150

Applications

  • Used as a flux in magnesium metal smelting, additive in aluminum electrolysis, coating material for optical lenses, pigment extender for titanium pigments, and fluorescent material for cathode ray screens

  • Applied in optical glass, ceramic industry, and electronic industry

  • Used in the manufacture of pottery and glass, as a flux for magnesium smelting, as a coating for lenses and filters in optical instruments, as an anti-refractive agent for optical lenses, and as a soldering agent

  • Solid-State Batteries: Magnesium fluoride can be used as a functional additive for solid-state electrolytes or as an interfacial modification layer. It helps reduce interfacial resistance, suppress lithium dendrite growth, and enhance the cycling stability and safety of solid-state batteries. With stable performance under a wide electrochemical window, it is suitable for high-voltage solid-state battery systems.

Packaging

Sample packaging: 100 g/bag, 500 g/bag, or 1 kg/bag

Storage Conditions

Keep container sealed and store in a cool, dry place away from moisture.


联系方式
手机:18268060973
手机:18268060375
手机:13235718865
微信扫一扫